| Property | Test Method | Requirement |
| Physical: | ||
| Tensile Strength | ASTM D 638 | 1200 min. |
| Elongation (%) | ASTM D 638 | 250 min. |
| Tensile Stress @ 200% elongation (psi) | ASTM D 412 | 2000 max. |
| Low Temperature Flex (-40° C) | AMS-DTL-23053 | No cracking |
| Heat shock (300° C, 4 hrs.) | AMS-DTL-23053 | No cracking |
| Heat resistance (250° C, 168 hrs.) | ||
| Elongation (%) | ASTM D 638 | 200 min. |
| Longitudinal change (%) | AMS-DTL-23053 | -20 max. |
| Electrical: | ||
| Dielectric strength (volts/mil) | ASTM D 876 | 200 min. |
| Volume resistivity (ohm-cm) | ASTM D 876 | 1.0 X 1011 min. |
| Chemical: | ||
| Copper mirror corrosion (175° C, 16 hrs.) | AMS-DTL-23053 | No corrosion |
| Water absorption (%) | ASTM D 570 | 0.5 max. |
| Fluid resistance (23° C, 24 hrs.) | ||
| Tensile strength (psi) | AMS-DTL-23053 | 1200 min. |
| Flammability | AMS-DTL-23053 | 15 sec. max. |
| Vacuum outgassing | ||
| TML, % | ASTM E 595 | 1.0 max. |
| CVCM, % | ASTM E 595 | 0.1 max. |
*For reference use only
| Nominal Size | ID Minimum (As Supplied) | ID Maximum (After Recovery) | Wall Thickness Nom (After Recovery) | |||
| Inches | MM | Inches | MM | Inches | MM | |
| 1/8″ | .125 | 3.2 | .062 | 1.6 | .031 | 0.80 |
| 3/16″ | .187 | 4.8 | .093 | 2.4 | .035 | 0.90 |
| 1/4″ | .250 | 6.4 | .125 | 3.2 | .035 | 0.90 |
| 3/8″ | .375 | 9.5 | .187 | 4.8 | .035 | 0.90 |
| 1/2″ | .500 | 12.7 | .250 | 6.4 | .035 | 0.90 |
| 3/4″ | .750 | 19.1 | .375 | 9.5 | .042 | 1.10 |
| 7/8″ | .875 | 22.2 | .437 | 11.1 | .049 | 1.20 |
| 1″ | 1.00 | 25.4 | .500 | 12.7 | .049 | 1.20 |
| 1.25″ | 1.25 | 31.8 | .625 | 15.9 | .055 | 1.40 |
| 1.5″ | 1.50 | 38.1 | .750 | 19.1 | .055 | 1.40 |